Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 2.275 - 3.448 GPa | 330.0 - 500.1 ksi | ASTM D882 |
Honeywell Capran® Emblem™ MT1500 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ MT1500 is a 0.60 mil (15 micron) biaxially oriented nylon 6 film with a metallized barrier coating well suited for high barrier packaging applications. Informati.. |
|||
Secant Modulus, TD | 2.586 - 3.448 GPa | 375.1 - 500.1 ksi | ASTM D882 |
Honeywell Capran® Oxyshield™ OEB (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of .. |
|||
Secant Modulus, TD | 2.586 - 3.448 GPa | 375.1 - 500.1 ksi | ASTM D882 |
Honeywell Capran® Oxyshield™ OEB (1.0 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Extra Barrier is a 1.00 (25micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film having excellent gas barrier through a broad range of relat.. |