Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 2.482 - 3.59 GPa | 360.0 - 521 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Secant Modulus, TD | 2.482 - 3.585 GPa | 360.0 - 520.0 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1200M Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1200M is a 0.48 mil (12 micron) biaxially oriented nylon 6 film with a polymeric coating which provides enhanced adhesion to a variety of inks, coatings, and adh.. |
|||
Secant Modulus, TD | 2.482 - 3.59 GPa | 360.0 - 521 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1200MT Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1200MT is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hy.. |