Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film  (discontinued **)

Category Polymer , Film , Thermoplastic , Nylon
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many solvents. It is also microwavable, making it an excellent choice for lidding stock. Applications: bag-on-box packaging, packaging for processed meats, cheese, meat snacks, coffee bricks, coffee bags, and pet food, agricultural bags, stand-up shampoo pouches, book covers and metallized balloons.Information provided by Honeywell.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0460 lb/in³
Yield Density
Water Vapor Transmission 9.31 - 12.42 g/m²/day
0.600 - 0.7998 g/100 in²/day
100°F / 100%RH); ASTM F1249
Oxygen Transmission Rate 9.31 - 13.97 cc/m²/day
0.600 - 0.8997 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Thickness 15.2 microns
0.600 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 60 - 90 %
60 - 90 %
ASTM D882
Film Elongation at Break, TD 60 - 90 %
60 - 90 %
ASTM D882
Secant Modulus, MD 2.41 - 3.93 GPa
350 - 570 ksi
ASTM D882
Secant Modulus, TD 2.482 - 3.59 GPa
360.0 - 521 ksi
ASTM D882
Coefficient of Friction 0.17 - 0.28
0.17 - 0.28
film to stainless steel; ASTM D1894
0.55 - 0.74
0.55 - 0.74
film to film; ASTM D1894
Tear Strength Test 1100 - 1500
1100 - 1500
graves tear, grams/mil (initial); ASTM D1004
Film Tensile Strength at Break, MD 234 - 303 MPa
34000 - 44000 psi
ASTM D882
Film Tensile Strength at Break, TD 193 - 303 MPa
28000 - 44000 psi
ASTM D882
Thermal Properties Metric English Comments
Shrinkage, MD 1.6 - 2.5 %
1.6 - 2.5 %
320°F / 160°C - 5 minutes; ASTM D1204
Shrinkage, TD 0.20 - 0.70 %
0.20 - 0.70 %
320°F / 160°C - 5 minutes; ASTM D1204
Optical Properties Metric English Comments
Haze <= 5.0 %
<= 5.0 %
ASTM D1003
Gloss 75 - 85 %
75 - 85 %
at 20°