Polymer Property : Secant Modulus, TD = 18.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.124 GPa
18.0 ksi
ASTM D882
Huntsman PE5082 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con..
Secant Modulus, TD 0.124 - 0.152 GPa
18.0 - 22.0 ksi
ASTM D882
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Secant Modulus, TD 0.124 GPa
18.0 ksi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film
9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F..
Secant Modulus, TD 0.124 GPa
18.0 ksi
ASTM D882
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin..
Secant Modulus, TD 0.124 - 1.18 GPa
18.0 - 171 ksi
Average value: 0.254 GPa Grade Count:19
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..
Secant Modulus, TD 0.124 - 0.333 GPa
18.0 - 48.3 ksi
Average value: 0.183 GPa Grade Count:23
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..