Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.124 - 0.152 GPa | 18.0 - 22.0 ksi | ASTM D882 |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |