Mechanical Properties Metric English Comments
Secant Modulus, TD 0.110 GPa
16.0 ksi
5%; ASTM D882
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend
The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film..
Secant Modulus, TD 0.110 GPa
16.0 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film
The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut..
Secant Modulus, TD 0.110 GPa
16.0 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging
The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th..
Secant Modulus, TD 0.110 GPa
16.0 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film
The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is..
Secant Modulus, TD 0.110 GPa
16.0 ksi
ASTM D882
Huntsman PE1753 EVA Film Extrusion  (discontinued **)
7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and ..
Secant Modulus, TD 0.110 GPa
16.0 ksi
50 µm (2 mil) film; ASTM D882
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol..
Secant Modulus, TD 0.110 GPa
16.0 ksi
ASTM D882
M. Holland Company LL217AA LLDPE  (discontinued **)
Features: High Clarity, Copolymer, Good ProcessabilityUses: Film, Cast FilmApprovals: FDA 21 CFR 177.1521Processing Method: Blown Film and Cast FilmInformation provided by M. Holland.