Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.910 GPa | 132 ksi | ASTM D882 |
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet
(discontinued **) Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str.. |
|||
Secant Modulus, TD | 0.910 GPa | 132 ksi | ASTM D 882 A |
Total 1285 HDPE film Applications: T-shirt sacks, trash can liners, merchandise bags, coex applicationsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics.. |
|||
Secant Modulus, TD | 0.910 GPa | 132 ksi | ASTM D 882 A |
Total 2285 HDPE Bimodal Film Resin Applications: T-shirt sacks, trash can liners, merchandise bags, multi-wall liner, deli wrapInformation provided provided by Total Petrochemicals. |
|||
Secant Modulus, TD | 0.910 GPa | 132 ksi | ASTM D 882 A |
Total 2287 HDPE Bimodal Film Resin Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe.. |
|||
Secant Modulus, TD | 0.910 GPa | 132 ksi | ASTM E111 |
LyondellBasell Alathon® L4434 High Density Polyethylene ApplicationsALATHON L 4434 is a medium molecular weight high density copolymer for use in blown film applications. Typical applications include blown film over pouches. Regulatory StatusL 4434 meet.. |