Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.300 GPa
43.5 ksi
ISO 527-3
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
Secant Modulus, TD 0.300 GPa
43.5 ksi
0.05-1.05%; ISO 527-3
Borealis Borstar® FB2230 LLDPE for Film
Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from ..
Secant Modulus, TD 0.300 GPa
43.5 ksi
ASTM D882-A
Borealis Himod™ FT3280 LDPE for Film
Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..