Polymer Property : Secant Modulus, TD = 0.117 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.117 GPa
17.0 ksi
ASTM D882
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o..
Secant Modulus, TD 0.117 GPa
17.0 ksi
ASTM D882
ExxonMobil Escorene® LD-318 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b..
Secant Modulus, TD 0.117 GPa
17.0 ksi
ASTM D882
ExxonMobil Escorene® LD-319 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b..
Secant Modulus, TD 0.117 GPa
17.0 ksi
ASTM D882
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light..
Secant Modulus, TD 0.117 GPa
17.0 ksi
ASTM D882
Huntsman PE1605 EVA Film Extrusion  (discontinued **)
6% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..
Secant Modulus, TD 0.117 GPa
17.0 ksi
ASTM D882
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD..