Mechanical Properties Metric English Comments
Secant Modulus, MD 0.172 GPa
24.9 ksi
0.01; ASTM D882
Eastman 184MF Polyethylene Film  (discontinued **)
Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character..
Secant Modulus, MD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Eastman 1840F Polyethylene  (discontinued **)
Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by..
Secant Modulus, MD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Eastman D4028-F Polyethylene  (discontinued **)
D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF..
Secant Modulus, MD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Eastman E6838-014F Polyethylene  (discontinued **)
E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta..
Secant Modulus, MD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Eastman E6838-899F Polyethylene  (discontinued **)
E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr..
Secant Modulus, MD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Eastman E6838-923F Polyethylene  (discontinued **)
E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit..
Secant Modulus, MD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Eastman E6838-997F Polyethylene  (discontinued **)
E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud..
Secant Modulus, MD 0.172 GPa
24.9 ksi
ASTM D882
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali..
Secant Modulus, MD 0.172 GPa
24.9 ksi
ASTM D882
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr..