Eastman E6838-014F Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman E6838-014F Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-contact applications E6838-014F meets the requirements of FDA regulations at 21 CFR 177.1520(c)(2.2) and may be used as a component of packages used for holding food during cooking. However, the polymer thickness in the form in which it contacts food shall not exceed 0.005 inches and contact is limited to non-alcoholic food because of a regulatory limitation for an adjuvant substance in this formulation.Information supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D4883
Thickness 32.0 microns
1.26 mil
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 21.0 MPa
3050 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ASTM D882
Film Elongation at Break, MD 350 %
350 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Secant Modulus, MD 0.172 GPa
24.9 ksi
1% Secant; ASTM D882
Secant Modulus, TD 0.179 GPa
26.0 ksi
1% Secant; ASTM D882
Coefficient of Friction 0.30
0.30
ASTM D1894
Elmendorf Tear Strength MD 380 g
380 g
Elmendorf Tear Strength TD 200 g
200 g
Elmendorf Tear Strength, MD 11.9 g/micron
302 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
ASTM D1922
Dart Drop 2.50 g/micron
63.5 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 21.0 MPa
3050 psi
ASTM D882
Film Tensile Strength at Break, TD 18.0 MPa
2610 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Gloss 70 %
70 %
at 45°; ASTM D2457
Transmission, Visible 25 %
25 %
ASTM D1746
Descriptive Properties Value Comments
Process Film