Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | 0.01; ASTM D882 |
Eastman 184MF Polyethylene Film
(discontinued **) Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | 1% Secant; ASTM D882 |
Eastman 1840F Polyethylene
(discontinued **) Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | 1% Secant; ASTM D882 |
Eastman D4028-F Polyethylene
(discontinued **) D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-014F Polyethylene
(discontinued **) E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-899F Polyethylene
(discontinued **) E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-923F Polyethylene
(discontinued **) E6838-923F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good clarit.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-997F Polyethylene
(discontinued **) E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | ASTM D882 |
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali.. |
|||
Secant Modulus, MD | 0.172 GPa | 24.9 ksi | ASTM D882 |
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr.. |