Polymer Property : Secant Modulus, MD = 1.131 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 1.131 - 1.551 GPa
164.0 - 225.0 ksi
ASTM D882
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film
Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf..