Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.207 - 1.551 GPa | 175.1 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Secant Modulus, MD | 1.207 - 1.551 GPa | 175.1 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Secant Modulus, MD | 1.207 - 1.551 GPa | 175.1 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Secant Modulus, MD | 1.207 - 1.551 GPa | 175.1 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Secant Modulus, MD | 1.379 - 1.551 GPa | 200.0 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Secant Modulus, MD | 1.131 - 1.551 GPa | 164.0 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf.. |
|||
Secant Modulus, MD | 1.310 - 1.551 GPa | 190.0 - 225.0 ksi | ASTM D882 |
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |