Mechanical Properties Metric English Comments
Secant Modulus, MD 1.207 - 1.551 GPa
175.1 - 225.0 ksi
ASTM D882
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Secant Modulus, MD 1.207 - 1.551 GPa
175.1 - 225.0 ksi
ASTM D882
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Secant Modulus, MD 1.207 - 1.551 GPa
175.1 - 225.0 ksi
ASTM D882
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Secant Modulus, MD 1.207 - 1.551 GPa
175.1 - 225.0 ksi
ASTM D882
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Secant Modulus, MD 1.379 - 1.551 GPa
200.0 - 225.0 ksi
ASTM D882
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell..
Secant Modulus, MD 1.131 - 1.551 GPa
164.0 - 225.0 ksi
ASTM D882
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film
Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf..
Secant Modulus, MD 1.310 - 1.551 GPa
190.0 - 225.0 ksi
ASTM D882
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film
Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..