Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.0278 - 0.170 GPa | 4.03 - 24.7 ksi | Average value: 0.101 GPa Grade Count:7 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Secant Modulus, MD | 0.160 - 0.170 GPa | 23.2 - 24.7 ksi | Average value: 0.162 GPa Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Liner Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Liner Grade". Each property range of values reported is minimum and max.. |