Mechanical Properties Metric English Comments
Shear Strength >= 9.00 MPa
>= 1310 psi
ISO 10123; Compressive, Steel pins and collars
Palm Labs Adhesives TURBO-LOCK SERIES 15 Anaerobic Thread Locking Compound
TURBO-LOCK 15 SERIES is a fast curing, large bolt, RED, high strength, anaerobic thread-locking compound for bonding and sealing threads. Prevents rusting of threads. It is highly resistance to heat..
Shear Strength 9.00 MPa
1310 psi
Short Beam
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..