COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate

Category Ceramic , Ceramic Matrix Composite , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer COI Ceramics
Trade Name Nextel™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air environments and are primarily used in both Aerospace and Gas Turbine applications.Ceramic Matrix System: Water Based Sol-Gel Processing, Versatile Matrix ChemistryTypical Applications for Oxide CMCs: Rotocraft Exhaust Systems, Advanced Thermal, Advanced CombustorInformation from COI Ceramics, Inc.
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Porosity 24 %
24 %
Mechanical Properties Metric English Comments
Tensile Strength 124 MPa
18000 psi
Tensile Stress 34.5 MPa

@Strain 0.100 %
5000 psi

@Strain 0.100 %
68.9 MPa

@Strain 0.200 %
10000 psi

@Strain 0.200 %
96.5 MPa

@Strain 0.300 %
14000 psi

@Strain 0.300 %
117 MPa

@Strain 0.400 %
17000 psi

@Strain 0.400 %
Tensile Modulus 31.0 GPa
4500 ksi
Shear Strength 9.00 MPa
1310 psi
Short Beam
Thermal Properties Metric English Comments
CTE, linear 4.80 µm/m-°C
2.67 µin/in-°F
Maximum Service Temperature, Air 650 °C
1200 °F
Descriptive Properties Value Comments
Nominal Fiber Volume (%) 48