Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 81.4 MPa | 11800 psi | ASTM D732 |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Shear Strength | 81.4 MPa @Thickness 15.7 mm |
11800 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |