Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 78.0 MPa | 11300 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK) AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava.. |
|||
Shear Strength | 78.0 MPa @Temperature 80.0 °C |
11300 psi @Temperature 176 °F |
In-Plane Shear, Wet; AiTM 1.0002 |
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process... |
|||
Shear Strength | 78.0 MPa @Temperature 22.0 °C |
11300 psi @Temperature 71.6 °F |
0° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, M60J Fiber Information provided by HexCel |
|||
Shear Strength | 78.0 MPa | 11300 psi | ASTM D732 |
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than AvaSpir.. |