Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 34.0 MPa | 4930 psi | |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Shear Strength | 34.0 MPa @Temperature 130 °C |
4930 psi @Temperature 266 °F |
90º, ILSS Short Beam, Wet; EN2563 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |
|||
Shear Strength | 34.0 MPa | 4930 psi | Overlap, Etched Al, Air at 149°C for 40 days |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 34.0 MPa @Temperature 24.0 °C, Time 1.04e+6 sec |
4930 psi @Temperature 75.2 °F, Time 288 hour |
Overlap, Cured for 7 days at 24°C |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 34.0 MPa | 4930 psi | |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |