Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 34.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 34.0 MPa
4930 psi
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Shear Strength 34.0 MPa

@Temperature 130 °C
4930 psi

@Temperature 266 °F
90º, ILSS Short Beam, Wet; EN2563
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber
Information provided by HexCel
Shear Strength 34.0 MPa
4930 psi
Overlap, Etched Al, Air at 149°C for 40 days
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Strength 34.0 MPa

@Temperature 24.0 °C,
Time 1.04e+6 sec
4930 psi

@Temperature 75.2 °F,
Time 288 hour
Overlap, Cured for 7 days at 24°C
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Strength 34.0 MPa
4930 psi
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin
Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Copyright © lookpolymers.com All Rights Reserved