3M Scotch-Weld™ 3747 Hot Melt Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 3747 Hot Melt Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose for wide variety of plastics, wood and lightweight metalsInformation provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity 4100 cP

@Temperature 191 °C
4100 cP

@Temperature 375 °F
Mechanical Properties Metric English Comments
Shear Strength 2.96 MPa
430 psi
On Douglas Fir
Peel Strength 3.51 kN/m
20.0 pli
on canvas
Thermal Properties Metric English Comments
Ring & Ball Softening Point 104 °C
219 °F
ASTM E28-99