Polymer Property : Shear Strength = 26.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 22.8 - 26.2 MPa
3300 - 3800 psi
ND Industries SuperGlue Methyl 330
Low-Medium Viscosity - General purpose metal surfaceMeets military spec Mil-A-46050C Type I Class II
Shear Strength 23.4 - 26.2 MPa
3400 - 3800 psi
CRS Overlap
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..