Polymer Property : Shear Strength = 2230 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 15.4 MPa
2230 psi
Shear Bond Holding Strength
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy
Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation.