Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 15.4 MPa | 2230 psi | Shear Bond Holding Strength |
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation. |