Mechanical Properties Metric English Comments
Shear Strength 22.1 MPa
3200 psi
Bond, Al to Al, RT Cure
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics
Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for..
Shear Strength >= 22.1 MPa
>= 3200 psi
Bond, Al to Al
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
Shear Strength >= 22.1 MPa
>= 3200 psi
Bond, Al to Al
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests
Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu..
Shear Strength 22.1 MPa
3200 psi
Overlap, Aluminum Oakite degrease
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 22.1 MPa
3200 psi
Overlap at 2 hrs after bonding
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 22.1 MPa
3200 psi
Overlap, CRS-MEK/Abrade/MEK, Cohesive/Adhesive Failure
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..
Shear Strength 22.1 MPa

@Temperature 24.0 °C
3200 psi

@Temperature 75.2 °F
Overlap, Etched Aluminum; ASTM D1002
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..