Mechanical Properties Metric English Comments
Shear Strength 95.0 MPa
13800 psi
ASTM D732
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr..
Shear Strength 95.1 MPa
13800 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope..
Shear Strength 95.1 MPa
13800 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Shear Strength 95.0 MPa
13800 psi
ASTM D732
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl..
Shear Strength 95.1 MPa
13800 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..
Shear Strength 95.1 MPa
13800 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Shear Strength 95.1 MPa
13800 psi
ASTM D732
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Shear Strength 95.0 MPa
13800 psi
0º, ILSS (Short Beam), RT, Dry; EN2563
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel