Polymer Property : Shear Strength = 136 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.938 MPa

@Temperature 82.0 °C,
Time 1.81e+6 sec
136 psi

@Temperature 180 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre..
Shear Strength 0.938 MPa
136 psi
Overlap, ABS, 50% RH
3M 4200 Marine Adhesive/Sealant Fast Cure
A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds to wood, gelcoat and fiberglass. It forms watertight, weather-resistant seals on joints an..
Shear Strength 0.938 MPa

@Thickness 12800 mm,
Time 295000 sec
136 psi

@Thickness 504 in,
Time 82.0 hour
Overlap, 1/8" Birch/Birch
3M Fastbond™ 4213-NF Industrial Adhesive
3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when..
Shear Strength 0.938 MPa

@Temperature 82.0 °C,
Time 1.81e+6 sec
136 psi

@Temperature 180 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre..