Material Notes:
3M™ Fastbond™ Industrial Adhesive 4213-NF is a white, water dispersed adhesive for bonding many fabrics, supported vinyl, wood, leather and most porous materials. Exhibits outstanding clarity when dry. Neither prone to discolor with age nor stain substrates. Note: Not recommended for exterior applications.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 54 - 60 %
54 - 60 %
Brookfield Viscosity 2500 - 5000 cP
2500 - 5000 cP
RVF #4 sp @ 20 rpm @ 62°C
Mechanical Properties Metric English Comments
Shear Strength 3.45 MPa
500 psi
Overlap, Wood/Wood
0.538 MPa

@Thickness 12800 mm,
Time 385000 sec
78.0 psi

@Thickness 504 in,
Time 107 hour
Overlap, 1/8" Birch/Birch
0.600 MPa

@Thickness 12800 mm,
Time 335000 sec
87.0 psi

@Thickness 504 in,
Time 93.0 hour
Overlap, 1/8" Birch/Birch
0.938 MPa

@Thickness 12800 mm,
Time 295000 sec
136 psi

@Thickness 504 in,
Time 82.0 hour
Overlap, 1/8" Birch/Birch
1.24 MPa

@Thickness 12800 mm,
Time 238000 sec
180 psi

@Thickness 504 in,
Time 66.0 hour
Overlap, 1/8" Birch/Birch
3.36 MPa

@Thickness 12800 mm,
Time 86400 sec
488 psi

@Thickness 504 in,
Time 24.0 hour
Overlap, 1/8" Birch/Birch
5.13 MPa

@Thickness 12800 mm,
Time -133000 sec
744 psi

@Thickness 504 in,
Time -37.0 hour
Overlap, 1/8" Birch/Birch
Peel Strength 1.40 - 2.63 kN/m

@Temperature 24.0 °C,
Time 173000 sec
8.00 - 15.0 pli

@Temperature 75.2 °F,
Time 48.0 hour
180°, Supported Vinyl/Wood
2.45 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
14.0 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
2.63 kN/m

@Temperature -37.0 °C,
Time 1.81e+6 sec
15.0 pli

@Temperature -34.6 °F,
Time 504 hour
180°, Canvas/Steel
2.63 kN/m

@Temperature 24.0 °C,
Time 86400 sec
15.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
3.51 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
20.0 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
4.21 kN/m

@Temperature 24.0 °C,
Time 259000 sec
24.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
4.73 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
27.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
5.26 kN/m

@Temperature 24.0 °C,
Time 432000 sec
30.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
6.14 kN/m

@Temperature 24.0 °C,
Time 605000 sec
35.0 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
6.14 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
35.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
Processing Properties Metric English Comments
Shelf Life 15.0 Month
15.0 Month
Descriptive Properties Value Comments
Appearance White (Wet) Clear (Dry)
Base Synthetic Resin