Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 77.2 MPa @Thickness 15.7 mm |
11200 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |
|||
Shear Strength | 77.0 MPa | 11200 psi | ASTM D732 |
Glastic Laminates/Shapes SG-200 High Strength/High Temperature Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-1. A superior replacement for epoxy-bonded mica in layer insulation applications. |
|||
Shear Strength | 77.0 - 88.0 MPa | 11200 - 12800 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Shear Strength | 77.0 - 88.0 MPa | 11200 - 12800 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |