Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 77.0 MPa | 11200 psi | ASTM D732 |
Glastic Laminates/Shapes SG-200 High Strength/High Temperature Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-1. A superior replacement for epoxy-bonded mica in layer insulation applications. |
|||
Shear Strength | 77.0 - 88.0 MPa | 11200 - 12800 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Shear Strength | 77.0 - 88.0 MPa | 11200 - 12800 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |