Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 77.2 MPa @Thickness 15.7 mm |
11200 psi @Thickness 0.620 in |
ASTM D732 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |