Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 10900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 75.0 MPa

@Temperature 75.0 °C
10900 psi

@Temperature 167 °F
In-Plane, Wet; EN6031
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel
Shear Strength 75.0 MPa
10900 psi
In-Plane, RT, Dry; EN6031
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel
Shear Strength 75.0 MPa
10900 psi
ILSS; EN2563
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm
Fiber mass: 150 g/m2Information provided by HexCel
Shear Strength 75.0 - 80.0 MPa
10900 - 11600 psi
IS 867-1963
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
Shear Strength >= 75.0 MPa
>= 10900 psi
2mm/min.; IS 867-1963
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded
Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins..
Shear Strength 75.0 - 90.0 MPa
10900 - 13100 psi
2mm/min.; IS 867-1963
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche..