Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/38%/UD150/CHS/460mm.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiber mass: 150 g/m2Information provided by HexCel
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Nominal Laminate
1.78 g/cc
0.0643 lb/in³
Fibre
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1500 MPa
218000 psi
EN2561
Flexural Yield Strength 1400 MPa
203000 psi
EN2562
Flexural Modulus 100 GPa
14500 ksi
EN2562
Shear Strength 75.0 MPa
10900 psi
ILSS; EN2563
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 85.0 - 90.0 °C
185 - 194 °F
DMA Onset
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0161
Fiber Volume (%) 52.4
Copyright © lookpolymers.com All Rights Reserved