Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.352 - 13.8 MPa | 51.0 - 2000 psi | Average value: 3.99 MPa Grade Count:7 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Shear Strength | 0.352 MPa | 51.0 psi | 2024 T3 Aluminum, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Shear Strength | 0.352 MPa | 51.0 psi | Overlap, Polypropylene |
3M 5010 Polyurethane Multi-Purpose Adhesive 3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, f.. |