JPJ Technologies PP H35S Homopolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer JPJ Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF JPJ Technologies PP H35S Homopolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP H35S is specifically developed for producing injection molding articles for general purpose applications. It gives consistent processability and high gloss in the products. Application: General use-Thin wall Miscellaneous, HousewaresInformation provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.8 MPa
4900 psi
ASTM D638
1% Secant Modulus 1500 MPa
218000 psi
ASTM D790A
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648