Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 6.00 - 33.2 g/micron | 152 - 843 g/mil | Average value: 22.2 g/micron Grade Count:15 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |