Polymer Property : Dart Drop = 6.00 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 6.00 g/micron
152 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent sealability, easy processability, excellent clarity.Applications: Blending resin for improved toughness.Data provided by the manufacturer.
Dart Drop 6.00 g/micron
152 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Eastman 5265 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Good optical properties, Superior impact strength, Low coefficient of friction, Good processability, High Slip, High Ant..
Dart Drop 6.00 g/micron
152 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Eastman 5267 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Excellent impact strength, Good optical properties, Good processability, High antiblock, No slipApplications:Laminations..
Dart Drop 6.00 g/micron
152 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par..
Dart Drop 6.00 g/micron
152 g/mil
ASTM D1709B
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging
Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene ..
Dart Drop 6.00 - 33.2 g/micron
152 - 843 g/mil
Average value: 22.2 g/micron Grade Count:15
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..
Dart Drop 6.00 - 22.1 g/micron
152 - 561 g/mil
Average value: 10.3 g/micron Grade Count:16
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Dart Drop 6.00 g/micron
152 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer.