Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 6.00 g/micron | 152 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 10A Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, easy processability, excellent clarity.Applications: Blending resin for improved toughness.Data provided by the manufacturer. |
|||
Dart Drop | 6.00 g/micron | 152 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Eastman 5265 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Good optical properties, Superior impact strength, Low coefficient of friction, Good processability, High Slip, High Ant.. |
|||
Dart Drop | 6.00 g/micron | 152 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Eastman 5267 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Excellent impact strength, Good optical properties, Good processability, High antiblock, No slipApplications:Laminations.. |
|||
Dart Drop | 6.00 g/micron | 152 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin
(discontinued **) Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par.. |
|||
Dart Drop | 6.00 g/micron | 152 g/mil | ASTM D1709B |
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene .. |
|||
Dart Drop | 6.00 - 33.2 g/micron | 152 - 843 g/mil | Average value: 22.2 g/micron Grade Count:15 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Dart Drop | 6.00 - 22.1 g/micron | 152 - 561 g/mil | Average value: 10.3 g/micron Grade Count:16 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Dart Drop | 6.00 g/micron | 152 g/mil | F 50; ASTM D1709/A |
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |