Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 6.56 - 11.8 g/micron | 167 - 300 g/mil | Average value: 8.00 g/micron Grade Count:8 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Dart Drop | 1.57 - 11.8 g/micron | 40.0 - 300 g/mil | Average value: 3.86 g/micron Grade Count:9 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |