Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 1.57 g/micron | 40.0 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a.. |
|||
Dart Drop | 1.57 g/micron | 40.0 g/mil | F50; ASTM D1709 |
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through .. |
|||
Dart Drop | 1.57 - 11.8 g/micron | 40.0 - 300 g/mil | Average value: 3.86 g/micron Grade Count:9 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Dart Drop | 1.57 g/micron | 40.0 g/mil | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade PETROTHENE NA272130 is a medium density polyethylene resin designed for overwrap film applications. NA272130 exhibits good film optics and high stiffness.Regulatory Status: NA272130 meets the requir.. |
|||
Dart Drop | >= 1.57 g/micron | >= 40.0 g/mil | ASTM D1709 |
ExxonMobil HD 7845.30 MMW Blown Film Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
Dart Drop | 1.57 g/micron | 40.0 g/mil | ASTM D1709 |
Huntsman Rexell® M3109 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer and FDA compliant.Features: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, multi-layer syste.. |
|||
Dart Drop | 1.57 - 59.1 g/micron | 40.0 - 1500 g/mil | Average value: 9.18 g/micron Grade Count:164 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Dart Drop | 1.57 g/micron | 40.0 g/mil | F50; ASTM D-1709 |
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom.. |