Polymer Property : Dart Drop = 40.0 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 1.57 g/micron
40.0 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LD-138 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin offering good clarity, toughness, and stiffness. Blown film made from this resin has good machinability in bag equipment a..
Dart Drop 1.57 g/micron
40.0 g/mil
F50; ASTM D1709
ExxonMobil Escorene® LD-117 MDPE Blown Overwrap Film Resin, Tough  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity and excellent stiffness. Film made from LD-117 can be used in overwrap applications and in push-through ..
Dart Drop 1.57 - 11.8 g/micron
40.0 - 300 g/mil
Average value: 3.86 g/micron Grade Count:9
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m..
Dart Drop 1.57 g/micron
40.0 g/mil
F<sub>50</sub>; ASTM D1709
LyondellBasell Petrothene® NA272130 Medium Density Polyethylene, Film Extrusion Grade
PETROTHENE NA272130 is a medium density polyethylene resin designed for overwrap film applications. NA272130 exhibits good film optics and high stiffness.Regulatory Status: NA272130 meets the requir..
Dart Drop >= 1.57 g/micron
>= 40.0 g/mil
ASTM D1709
ExxonMobil HD 7845.30 MMW Blown Film Resin
Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc..
Dart Drop 1.57 g/micron
40.0 g/mil
ASTM D1709
Huntsman Rexell® M3109 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer and FDA compliant.Features: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, multi-layer syste..
Dart Drop 1.57 - 59.1 g/micron
40.0 - 1500 g/mil
Average value: 9.18 g/micron Grade Count:164
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..
Dart Drop 1.57 g/micron
40.0 g/mil
F50; ASTM D-1709
ExxonMobil Escorene® HD-7835 MMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A medium molecular weight HDPE blown film resin. Films made from the HD-7835 exhibit an excellent stiffness balance. HD-7835 is particularly recom..