Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 130 g
130 g
Eastman 1810F Polyethylene  (discontinued **)
Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt..
Elmendorf Tear Strength TD 130 g
130 g
Eastman 1830F Polyethylene  (discontinued **)
Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and..
Elmendorf Tear Strength TD 130 g
130 g
Eastman D4004-F Polyethylene  (discontinued **)
Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o..
Elmendorf Tear Strength TD 130 g
130 g
Eastman D4008-F Polyethylene  (discontinued **)
Polyethylene D4008-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness and clarityList of Applications: Food packagingFood-contac..
Elmendorf Tear Strength TD 130 g
130 g
Eastman E6838-969F Polyethylene  (discontinued **)
E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap...
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
LyondellBasell Petrothene® NA960000 Low Density Polyethylene
ApplicationsPETROTHENE NA960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA960 exhibits good unif..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
LyondellBasell Petrothene® NA960070 Low Density Polyethylene
ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
LyondellBasell Petrothene® NA960083 Low Density Polyethylene
ApplicationsPETROTHENE NA 960 is a series of resins designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 960 exhibits good un..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation. Availability: Africa & M..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin
Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin
Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Elmendorf Tear Strength TD 130 g
130 g
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade
DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D1922
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b..
Elmendorf Tear Strength TD 130 g
130 g
ASTM-D1922
Braskem LD7000A LDPE Blown Film Extrusion Polyethylene
LD7000A is a low-density polyethylene produced by the high pressure process in an autoclave reactor. It is developed for the manufacturing of extruded films. It has high mechanical and impact streng..
Elmendorf Tear Strength TD 130 g

@Thickness 0.0381 mm
130 g

@Thickness 0.00150 in
ASTM D-1922
Bapolene® 107A Low Density Polyethylene Film Extrusion Resin
Bapolene® 107A is an LDPE for blown film. It contains 3400 ppm antiblock additive. This product meets the Food and Drug Administration requirements of 21CFR177.1520.Applications: General purpose p..
Elmendorf Tear Strength TD 130 g
130 g
ASTM D-1922
Bapolene® 200B Polyethylene, Film Extrusion
Bapolene 200B is a low density polyethylene for blown film applications requiring superior clarity. It complies with US FDA 21CFR177.1520.Applications: General purpose, bakery, flexible, medical an..
Elmendorf Tear Strength TD 130 g
130 g
Eastman D4052-F Polyethylene  (discontinued **)
D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance...
Elmendorf Tear Strength TD 130 g
130 g
Eastman E6838-975F Polyethylene  (discontinued **)
E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film..