Material Notes:
Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList of Applications: Food packagingFood-contact applicationsInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D4883
Thickness 38.0 microns
1.50 mil
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 33.0 MPa
4790 psi
ASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ASTM D882
Film Elongation at Break, MD 200 %
200 %
ASTM D882
Film Elongation at Break, TD 800 %
800 %
ASTM D882
Secant Modulus, MD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Secant Modulus, TD 0.274 GPa
39.7 ksi
1% Secant; ASTM D882
Elmendorf Tear Strength MD 550 g
550 g
Elmendorf Tear Strength TD 130 g
130 g
Elmendorf Tear Strength, MD 14.5 g/micron
368 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 3.40 g/micron
86.4 g/mil
ASTM D1922
Dart Drop 2.90 g/micron
73.7 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 33.0 MPa
4790 psi
ASTM D882
Film Tensile Strength at Break, TD 22.0 MPa
3190 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 8.5 %
8.5 %
ASTM D1003
Gloss 60 %
60 %
at 45°; ASTM D2457
Descriptive Properties Value Comments
Process Film