Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 941 MPa | 137000 psi | at Center, Transverse |
International Mold Steel P20 Plastic Mold Steel P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel.
Information provided by International Mold Steel. |