Material Notes:
P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel. Information provided by International Mold Steel.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28 - 32
28 - 32
Tensile Strength, Ultimate 932 MPa
135000 psi
at Center, Longitudinal
941 MPa
137000 psi
at Center, Transverse
981 MPa
142000 psi
at Surface, Longitudinal
981 MPa
142000 psi
at Surface, Transverse
Tensile Strength, Yield 804 MPa
117000 psi
at Center, Transverse
873 MPa
127000 psi
at Surface, Transverse
873 MPa
127000 psi
at Surface, Longitudinal
873 MPa
127000 psi
at Center, Longitudinal
Impact 3.0
3.0
(kgf m/cm<sup>2</sup>), Impact Toughness at Center, Transverse
3.2
3.2
(kgf m/cm<sup>2</sup>), Impact Toughness at Surface, Transverse
3.6
3.6
(kgf m/cm<sup>2</sup>), Impact Toughness at Center, Longitudinal
5.2
5.2
(kgf m/cm<sup>2</sup>), Impact Toughness at Surface, Longitudinal