Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 901 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 6.21 MPa
901 psi
Momentive Performance Materials RTV157 Gray Adhesive Sealant, High Strength Paste
One-part cure. Typical uses: High strength adhesive; use for gasketing, aircraft maintenance, and electrical insulation.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of..
Tensile Strength, Ultimate 6.21 - 7.59 MPa
901 - 1100 psi
Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020)
Uncured, unsupported silicone rubber with a thickness of 0.020 in ± 0.002 (0.51 mm ± 0.051) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.08 mm) polyethylene interleave..
Copyright © lookpolymers.com All Rights Reserved