Polymer Property : Tensile Strength, Ultimate = 1100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 6.21 - 7.59 MPa
901 - 1100 psi
Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020)
Uncured, unsupported silicone rubber with a thickness of 0.020 in ± 0.002 (0.51 mm ± 0.051) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.08 mm) polyethylene interleave..