Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 65.0 - 86.0 MPa | 9430 - 12500 psi | Average value: 80.4 MPa Grade Count:7 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Tensile Strength, Ultimate | 53.4 - 86.0 MPa | 7750 - 12500 psi | Average value: 66.8 MPa Grade Count:5 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |